EN16 engineering steel, also known as 605m36, comes as rolled (no heat
treatment) or hardened and tempered to the ‘T’ condition.
EN16 displays excellent ductility and shock resistance. As such itis a good choice for a
range of general engineering uses.
Element | COMPOSITION |
---|---|
C | 0.35% |
Si | 0.30% |
Mn | 1.50% |
S | 0.030% |
P | 0.025% |
Mo | 0.25% |